Introduction
Ti-deoxidized pure nickel welding wire is used for welding nickel 210 or nickel 201, and the welding of different materials including nickel alloy with stainless steel or ferrite steel. It can also be used as transition layer when surfacing Cu-Ni alloy on steel.
C | Si | Ni | Ti | Mn | Fe | Al |
0.06 | 0.4 | 95.5 | 3 | 0.3 | 0.1 | 0.5 |
Tensile Strength | Yield Strength | Elongation |
460MPa | 260MPa | 0.28 |